Abstract The present study is focused on the metallurgical factors inced ring high-temperature operation of a pipeline that resulted in its short-time failure. The pipeline is used as superheater in a lignite power-plant unit and is constructed by an array of steel tubes jointed together by circumferential weldments. Systematic recording of data over one year of service indicated that local material’s failures were occurring, on an average, every 15 days and localised either at curved areas of the tubes, or in the neighbourhood of circumferential weldments. Visual inspection, macrographic examination and microscopic observations of representative failed parts revealed microstructural features indicative of creep rupture. In both cases, the material failed e to the rapid growth and coalescence of creep voids, initiated at a service temperature equal to 43% of the steel melting point.Article Outline 1. Background information and service history 2. Experimental techniques 3. Results 3.1. Failure at the curved areas of the pipeline 3.2. Failure in the neighbourhood of welding seams4. Discussion and conclusions Acknowledgements Referenceshttp://www.sciencedirect.com/science?_ob=ArticleURL&_udi=B6V2X-4TGXPGN-3&_user=10&_rdoc=1&_fmt=&_orig=search&_sort=d&_docanchor=&view=c&_searchStrId=1106784718&_rerunOrigin=google&_acct=C000050221&_version=1&_urlVersion=0&_userid=10&md5=4c3bc59690b1bb7685c76ad2c4052fbf

声明声明:本网页内容为用户发布,旨在传播知识,不代表本网认同其观点,若有侵权等问题请及时与本网联系,我们将在第一时间删除处理。E-MAIL:11247931@qq.com